Construction Technology And Precautions Of Exterior Stone Paint

date:2017-04-05
I believe that many people do not understand the real stone paint, people say that the external walls of real stone paint construction technology and paint the same construction process, in fact, this is a misunderstanding, the external walls of stone construction process seems simple, in fact, there are many need to pay attention The place. Therefore, the next Xiaobian to tell you what is really stone and the external walls of real stone paint construction process and precautions.

真石漆

 

What is really stone paint
 
Really stone paint is a decorative effect resembles the marble, granite paint, prepared by the natural color of various colors of natural stone, with natural and natural natural color, giving elegant, harmonious, solemn beauty, suitable for all kinds of buildings Indoor and outdoor decoration.
 
The construction technology of the external wall stone
 
Wall selection and wall finishing: for concrete or cement inside and outside the wall and brick walls, as well as asbestos cement board, plank, gypsum board, polyurethane foam board and other substrates. Construction substrate surface layer should be smooth, clean, no cracks.

 

防石漆

 

Construction Technology of Exterior Stone Paint
 
Spray the base oil and real stone paint: alkali-resistant primer or wall treatment agent back cover again, dry and then use a special spray gun painted real stone paint, spray one or two times (can also scratch), recoat interval of 2 hours or more.
 
Construction Technology of Exterior Stone Paint
 
Polished: 400 - 600 mesh sandpaper, gently wipe the surface of the real stone can be raised sand. Note that the force can not be too fierce, otherwise it will damage the film, causing the bottom of the loose, serious will cause poor adhesion, really stone off.
 
Construction Technology of Exterior Stone Paint
 
Spraying the surface oil: the next pot spray gun, pressure 4-7 kg / cm, the construction of not less than 10 ℃, spray twice, interval of 2 hours, the thickness of about 30 microns, completely dry to 7 days.
 
Facade of the real stone paint construction matters one
 
Construction, the scaffolding should be about 30cm from the wall, so as not to affect the decorative effect;

 

真石漆

 

Precautions for construction of external walls
 
Do not spray parts and objects, the application of baffle or paper, etc. separated;
 
Precautions for construction of external walls
 
Construction temperature should be higher than 5 ℃, wind is greater than 4 when not suitable for construction. The main coating spray within 24 hours should avoid rain and snow;
 
Precautions for construction of external walls
 
Oily primer, overcoat is a flammable dangerous goods, construction should be strictly prohibited fireworks;
 
Precautions for construction of external walls
 
In the construction process, is strictly prohibited in the use of materials in the water diluted;
 
Precautions for construction of external walls
 
The lower the temperature when the same wall to survive, or even the same batch after a long time construction will appear a slight color problems.